4.7 Article

Effect of fibre orientation on the fatigue behaviour of a short glass fibre reinforced polyamide-6

期刊

INTERNATIONAL JOURNAL OF FATIGUE
卷 29, 期 2, 页码 199-208

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.ijfatigue.2006.04.001

关键词

short glass fibre reinforced polyamide-6; fatigue strength; fibre orientation; Tsai-Hill criterion

向作者/读者索取更多资源

The effect of fibre orientation on the fatigue Strength of a short glass fibre reinforced polyamicic-6 has been investigated. Tension-tension axial fatigue tests were conducted with specimens extracted from injection moulded plates. Specimens were cut Out of plates with different orientations with respect to the longitudinal axis of plates, and therefore displayed different orientations of the reinforcing fibres. Results are presented in the form of S - N curves, showing the variation of the fatigue strength as a function of the specimen orientation. The experimental data, both tensile and fatigue tests, have been compared with values predicted by a failure criterion derived from the Tsai-Hill formula. The influence oil the fatigue lives of the fibre orientation distribution in the thickness of the specimen is discussed. (c) 2006 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据