ANALYTICA CHIMICA ACTA
卷 587, 期 2, 页码 263-271出版社
ELSEVIER
DOI: 10.1016/j.aca.2007.01.039
关键词
ion-imprinted polymers; preconcentration; chelating ligand; uranium recovery; analysis; seawater
Uranyl ion-imprinted polymeric (IIP) resins were prepared by dissolving stoichiometric amounts of uranyl nitrate and selected chelating ligands, viz. salicylaldoxime, catechol, succinicacid, 5,7-dichloroquinoline-8-ol and 4-vinyl pyridine in 2-methoxy ethanol (porogen) and copolymerizing thermally in the presence of 2-hydroxyethylmethacrylate (HEMA) and ethyleneglycol-dimethacrylate (EGDMA), using 2,2'-azobisisobutyronitrile (initiator). Again, IIP resins were also prepared on similar lines by utilizing ternary [uranium-non-vinylated ligand-vinylated ligand (4-vinyl pyridine)] complexes. Non-imprinted polymeric resins were identically prepared in both cases without the use of uranyl imprint ion. The percent enrichment and retention capacity studies showed significant imprinting effect in all cases. However, ion-imprinted polymeric resins formed with succinic acid (SA) or 5,7-dichloroquinoline-8-ol (DCQ) and 4-vinylpyridine (VP) alone gave quantitative enrichment and various parameters that influence the enrichment and elution were then optimized. The percent enrichment of uranium from synthetic seawater solutions was found to be 25.0 +/- 0.5 and 83.0 +/- 0.8 for SA-VP and DCQ-VP systems, respectively. The DCQ-VP-based IIP resins were successfully tested for the recovery of uranium from real seawater samples. (c) 2007 Elsevier B.V All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据