Dynamic TGA-FTIR studies on the thermal stability of lithium/graphite with electrolyte in lithium-ion cell

期刊

JOURNAL OF POWER SOURCES
卷 167, 期 2, 页码 515-519

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jpowsour.2007.02.029

关键词

TGA-FTIR; graphite anode; SEI film; thermal runaway; Li-ion cell

向作者/读者索取更多资源

Graphite anode could initialize the thermal runaway of lithium-ion cells due to its spontaneous exothermic reactions above the critical temperature. In order to explore the mechanisms of these reactions, a series of experiments were carried out with on-line coupled thermogravimetric analyser-Fourier transform infrared spectrometer (TGA-FTIR). The reactions under study essentially involved metallic lithium reacting with electrolyte and the thermal decomposition of natural graphite GDR at various states of charge (SOC). It is found that metallic lithium reacts with ethylene carbonate (EC) violently at around 180 degrees C producing CO, and dilithio butylene dialkoxide which could further react with LiPF6 and/or PF5 to produce POF3. At the relatively low temperature (about 60 degrees C), CO2 produced from both 0% SOC and 100% SOC GDR samples is attributed to the decomposition of organic compounds in solid electrolyte interface (SEI) film. In addition, the amount of POF3 produced from 0% SOC GDR sample is more than that from 100% SOC GDR sample. Further, fully intercalated GDR sample shows a structural collapse, a solid-state exothermic reaction at similar to 260 degrees C. Based on the TGA-FTIR results obtained from these exothermic reactions, detailed thermal decomposition paths are proposed in this paper. (C) 2007 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据