Shear-induced adhesive failure of a rigid slab in contact with a thin confined film

期刊

EUROPEAN PHYSICAL JOURNAL E
卷 23, 期 2, 页码 175-183

出版社

SPRINGER
DOI: 10.1140/epje/i2007-10171-x

关键词

-

向作者/读者索取更多资源

A rigid-glass prism (square or rectangular base, rectangular cross-section) is sheared off a thin film of silicone elastomer bonded to a glass plate by applying a tangential force at various distances above the prism/elastomer interface. At a given tangential force, the prism starts to slide on the elastomeric film. As the sliding velocity, thus the frictional force, is progressively increased, an elastic instability develops at the interface that results in the formation of numerous bubbles. These bubbles, the lateral dimension of which is comparable to the thickness of the film, move across the interface with speeds 1000 times faster than the overall sliding speed of the glass prism against the PDMS film. It is found that the glass prism continues to slide on the elastomeric film as long as the applied shear stress is less than a critical value. During sliding, however, a normal stress is developed at the interface that decays from the front (i.e. where the force is applied) to the rear end of the prism. When the normal stress reaches a critical value, the prism comes off the film. The critical shear stress of fracture increases with the modulus of the film, but decreases with the thickness following a square root relationship, as is the case with the removal of rigid punches from thin elastomeric films by normal pull-off forces.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据