All-ceramic dental restorations exhibit enhanced esthetics and biocompatibility as compared to traditional metal-based prosthesis. However, long-term fatigue and subcritical crack growth in the presence of water and cyclic loading can decrease the strength of ceramic components over time. We investigated the cyclic fatigue in water of three dental materials currently used as frameworks in all-ceramic restorations: a 3 mol%-yttria partially stabilized zirconia (3Y-TZP, Cercon, Degudent GmbH), a Al2O3-ZrO2-Glass composite (Inceram-Zirconia, Vita Zahnfabrik GmbH) and a Li(2)O(.)2SiO(2), glass ceramic (Empress 2, Ivoclar Vivadent AG). Fatigue and fast fracture tests were performed to determine the Weibull distribution of lifetime and initial mechanical strength for each framework component. In spite of its noticeable susceptibility to fatigue in water, the 3Y-TZP material was found to be particularly suitable for the preparation of posterior all-ceramic bridges due to its high initial mechanical strength. Guidelines are provided for the selection of materials and the design of all-ceramic posterior bridges exhibiting lifetime longer than 20 years under severe wet and cyclic loading conditions. (c) 2007 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据