Fabrication and characterization of Bi0.4Te3.0Sb1.6 thin films by flash evaporation method

期刊

JOURNAL OF ALLOYS AND COMPOUNDS
卷 441, 期 1-2, 页码 246-250

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2006.09.136

关键词

thin film; flash evaporation; thermoelectric; annealing

向作者/读者索取更多资源

Bi0.4Te3.0Sb1.6 thin films on glass substrates are fabricated by a flash evaporation method. In order to enhance the transport properties of the thin films, annealing in argon ambient at atmospheric pressure is carried out for 1 h in the temperature range from 200 to 400 degrees C. The structure of the thin films, in terms of homogeneous composition and crystallinity, is investigated by energy dispersive X-ray spectroscopy and X-ray diffraction, respectively. The microstructure of the thin films is examined using scanning electron microscopy. We confirm that as-deposited Bi0.4Te3.0Sb1.6 thin films have a mostly homogeneous structure except for a few extra stuck particles. At higher annealing temperatures, the crystallinity of the thin films is improved and the size of crystal grains increases to the same size as the film thickness. However, excessive high annealing temperatures cause porous thin films due to the evaporation of tellurium. The transport properties of the thin films, in terms of the electrical resistivity, the Seebeck coefficient and the thermoelectric power factor are determined at room temperature. By optimizing the annealing conditions, it is possible to obtain a high-performance thin film with a thermoelectric power factor of 12.2 mu W cm(-1) K-2. We consider that the performance of the thin films is enhanced for optimized annealing because of reductions in the importance of grain boundary scattering. (C) 2006 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据