4.7 Article

Bioleaching of iron from highly contaminated kaolin clay by Aspergillus niger

期刊

APPLIED CLAY SCIENCE
卷 37, 期 3-4, 页码 251-257

出版社

ELSEVIER
DOI: 10.1016/j.clay.2007.01.010

关键词

kaolin; bioleaching; Aspergillus niger; iron removal

向作者/读者索取更多资源

Kaolin is a clay mineral that has a wide application in the industry specially, in paper, ceramic, and porcelain manufacturing. One of the most important factors that affects the value of this raw material is its brightness. Unfortunately, with the iron oxides deposit on mineral particles during kaolin formation, much of this clay has become unusabte for industries. So, several chemical methods have been applied in mineral processing plants to reduce these contaminants, but finding a more sustainable approach like biological methods have always attracted a great attention. In this work bioleaching of iron from a highly contaminated kaolin sample was carried out using two different strains of Aspergillus niger, and the effects of strain type, pulp density, and time of clay addition on the iron retrieval were investigated by employing a 2 3 full factorial design. Finally, it is concluded that strain type has the most significant effect on the response; also, the highest removal extent was 42.8% that was obtained by using the strain isolated from pistachio shell, and at the pulp density of 20 g/l when the clay was added at the beginning of the experiments. (c) 2007 Elsevier B.V All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据