Cbrysotile from Thetford, Quebec, was heated at constant temperature in quench furnaces from 200 to 1000 degrees C for 4 to 720 h, and the products were analyzed by XRD and optical microscopy. XRD patterns for chrysotile from Thedford, Jeffrey Quebec, and New Idria, California, heated for up to 8 It at constant temperatures from 400 to 800 degrees C in hydrothermal diamond-anvil cells, were obtained at 300 s intervals by using synchrotron radiation. The studies show that differences in the decomposition temperatures of chrysotile reported in the literature can be explained by differences in the temperatures, time at temperature, particle size, and partial pressure of water. Chrysotile heated for 30 days is destroyed between 475 and 500 degrees C, whereas chrysotile heated to 800 T survives for only minutes. A prograde heating experiment, consistent with the literature, shows chrysotile destruction beginning at 600 degrees C and completed at 750 degrees C, demonstrating that such experiments should not be used to establish temperatures of thermal stability. Forsterite forms readily at 600 degrees C when water is retained transiently in the decomposition products, but does not form after 4 h of heating samples of small fiber size and high surface area from which water is readily lost. When water is retained in the sample chamber during heating to 800 degrees C over 4 h, a rapid destruction of chrysotile and formation of forsterite was observed, followed by the appearance and later destruction of the intermediate reaction products talc, a tridymite-like phase, and anthophyllite; enstatite appearance coincides with the destruction of the tridymite-like phase and talc. In quench experiments, a 10+ angstrom phase is observed between 500 and 600 degrees C, and talc is observed between 587 and 800 degrees C. The optical properties of the run products between 600 and 900 degrees C are highly variable, with a range in the index of refraction perpendicular to length of up to 0.06 and a minimum index of refraction 0.03 below the starting material in fibers in the 650 degrees C run product; the variability reflects the inhomogeneity in products and reactants in this temperature range. In quench experiments, the intensity of the XRD patterns of chrysotile decreased on heating between 200 and 400 degrees C, and increased at 450 degrees C, demonstrating recrystallization of chrysotile. A gradual heating experiment showed a similar pattern with the lowest intensities at 250 degrees C and maximum intensities at 550 degrees C. The two types of chrysotile reported in the literature may reflect simply the presence of chrysotile of different particle sizes. Chrysotile may also possess a spectrum of stabilities due to variable strain energies of curvature. The presence of a tridymite-like phase supports the formation of a Si-rich dehydroxylate II. The absence of forsterite and chrysotile in brake-wear debris reflects the high temperature and disaggregated fiber bundles resulting from friction.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据