We present dimensional and density changes in an aging plutonium alloy enriched with 7.3 at.% of Pu-238 and reference alloys of various ages. After 45 equivalent years of aging, the enriched alloys at 35 degrees C have swelled in length by 0.048-0.052% and now exhibit a near linear dimensional increase, without void swelling. Based on X-ray diffraction measurements, the lattice expansion by self-irradiation appears to be the primary cause for dimensional changes during the initial 2-3 years of aging. Following the initial transient, the density change is primarily cause by a constant helium in-growth rate as a result of a-particle decay. Published by Elsevier B.V.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据