Alkali activation of fly ash:: Effect of the SiO2/Na2O ratio Part I:: FTIR study

期刊

MICROPOROUS AND MESOPOROUS MATERIALS
卷 106, 期 1-3, 页码 180-191

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.micromeso.2007.02.055

关键词

fly ash; alkaline activation; FTIR; soluble silica; aluminosilicate; zeolites

向作者/读者索取更多资源

In this paper the main reaction products formed in alkali activated fly ash systems have been studied by using Infrared Spectroscopy. The main variables of work were: soluble silica content in the alkaline activating solution (0% SiO2; 1.62% SiO2; 5.40% SiO2 and 9.07% SiO2) and thermal curing time (8 h, 60 and 180 days). The results obtained have shown that the main reaction product formed in all cases was an alkaline aluminosilicate-type gel regarded to be a zeolite precursor. By means of the Infrared Spectroscopy it has been shown that there is an asymmetric stretching band (T-O), associated with that aluminosilicate-type gel, which can be interpreted in terms of that gel showing two different types of Si-O bonds: bridge and terminal bonds. The presence of soluble silica modifies reaction kinetics and prompts the formation of more Si-rich gels with a higher percentage of bridge bonds. The presence of soluble silica also affects the rate of crystallization and the type of zeolites formed (Na-Chabacite, zeolite Y, zeolite P). Finally when the thermal curing time increases, the gel undergoes polymerization and its structure becomes highly ordered (with a predominance of bridge over terminal bonds) (c) 2007 Elsevier Inc. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据