Gd2O3 : Eu3+; phosphor; homogeneous precipitation; nanoparticle; photoluminescence
Europium-activated Gd2O3 phosphor powders were prepared by homogeneous precipitation method, and the effects of urea concentration and reaction temperature on the morphology of precursor powders were investigated. The synthesized powders were characterized by means of XRD, SEM, TG/DTA and FT IR. The synthesis of gadolinium carbonate compounds was carried out using this method from relatively high concentrations of gadolinium salt and urea for the first time. Two kinds of powders formed were the crystalline Gd-2(CO3)(3)center dot 2.5H(2)O and Gd2O(CO3)(2)center dot H2O phases, which were mainly affected by reaction temperature. Namely, the Gd-2(CO3)(3)center dot 2.5H(2)O phase was formed at 80-90 degrees C, and the Gd2O(CO3)(2)center dot H2O at 100 C. The morphology of Gd-2(CO3)(3)center dot 2.5H(2)O phase was plate-like. And the powders of Gd2O(CO3)(2)center dot H2O phase showed the rectangular plate-like morphology. In order to synthesize the manometer-sized precursor powders using the homogeneous precipitation technique, it was found that EDTA/[Gd + Eu] mole ratio should be larger than 7.5 x 10(-3) M, corresponding to 15 mol% of total cation concentration. The manometer-sized precursor showed the amorphous-like pattern. The thermal decomposition behaviors of the three kinds of gadolinium carbonate compounds were also investigated. The thermal stability had the following order: Gd2O(CO3)(2)center dot H2O > Gd-2(CO3)(3)center dot 2.5H(2)O > amorphous phase. (C) 2007 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据