4.8 Article

Tensile Tests on Individual Single-Walled Carbon Nanotubes: Linking Nanotube Strength with Its Defects

期刊

ADVANCED MATERIALS
卷 22, 期 36, 页码 4071-4075

出版社

WILEY-V C H VERLAG GMBH
DOI: 10.1002/adma.201001463

关键词

-

资金

  1. International Center for Materials Nanoarchitectonics (MANA) of the National Institute for Materials Science (NIMS), Tsukuba, Japan

向作者/读者索取更多资源

The ultimate tensile strength of individual single-walled carbon nanotubes (CNTs) is measured in a high-resolution transmission electron microscopy equipped with a conducting atomic force microscopy unit. The values are correlated to every tube's structural details. The strength of similar to 100 GPa, approaching the theoretical limit for defect-free CNTs, is documented in tubes without visible defects; for those with spatially separated stepwise pentagon-heptagon defects, determining the breaking sites, it reduces to 40-70 GPa.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据