4.1 Article

Effect of soft drinks on the physical and chemical features of nickel-titanium-based orthodontic wires

相关参考文献

注意:仅列出部分参考文献,下载原文获取全部文献信息。
Article Dentistry, Oral Surgery & Medicine

Effects of a diamond-like carbon coating on the frictional properties of orthodontic wires

Takeshi Muguruma et al.

ANGLE ORTHODONTIST (2011)

Article Dentistry, Oral Surgery & Medicine

Why do nickel-titanium archwires fracture intraorally? Fractographic analysis and failure mechanism of in-vivo fractured wires

Spiros Zinelis et al.

AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS (2007)

Article Dentistry, Oral Surgery & Medicine

Effect of soft drinks on proximal plaque pH at normal and low salivary secretion rates

Ann-Katrin Johansson et al.

ACTA ODONTOLOGICA SCANDINAVICA (2007)

Article Dentistry, Oral Surgery & Medicine

Effect of acidic food and drinks on surface hardness of enamel, dentine, and tooth-coloured filling materials

S Wongkhantee et al.

JOURNAL OF DENTISTRY (2006)

Article Engineering, Biomedical

Corrosion resistance of stressed NiTi and stainless steel orthodontic wires in acid artificial saliva

HH Huang

JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A (2003)

Article Engineering, Biomedical

Hydrogen embrittlement of Ni-Ti superelastic alloy in fluoride solution

K Yokoyama et al.

JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A (2003)

Article Engineering, Biomedical

Delayed fracture of beta titanium orthodontic wire in fluoride aqueous solutions

K Kaneko et al.

BIOMATERIALS (2003)

Article Dentistry, Oral Surgery & Medicine

Permeability and morphology of dentin after erosion induced by acidic drinks

C Prati et al.

JOURNAL OF PERIODONTOLOGY (2003)

Article Engineering, Biomedical

Measuring the elastic properties of fine wire

CT Fallen et al.

JOURNAL OF BIOMEDICAL MATERIALS RESEARCH (2001)

Article Engineering, Biomedical

Degradation and fracture of Ni-Ti superelastic wire in an oral cavity

K Yokoyama et al.

BIOMATERIALS (2001)