4.7 Article

Effect of total dopant concentration and dopant ratio on conductivity of (DyO1.5)(x)-(WO3)(y)-(BiO1.5)1-x-y

期刊

ACTA MATERIALIA
卷 58, 期 2, 页码 355-363

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.actamat.2009.08.072

关键词

Solid electrolytes; Bismuth oxide; Lattice parameter; Conductivity; Total dopant concentration

资金

  1. National Aeronautics and Space Administration (NASA) [NAG3-2930]
  2. Florida Institute for Sustainable Energy (FISE)

向作者/读者索取更多资源

Dysprosium- and tungsten-stabilized bismuth oxide (DWSB) electrolytes were developed to achieve higher conductivity. With double doping, stabilization of the cubic phase was achieved with as little as 12 mol.% total dopant concentration, resulting in higher conductivity. The conductivity of DWSB electrolytes increased linearly as the total dopant concentrations decreased with fixed dopant ratio. Overall, DWSB has a closer inherent structure to pure delta-Bi2O3 than any singly doped compositions. Both lattice parameter and conductivity linearly extrapolate with total dopant concentration to that of pure delta-Bi2O3, resulting in the ability to stabilize delta-phase at lower dopant concentration, and thus achieving higher conductivity. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据