Nanograined (grain size 10 nm) ZnO films with various Co contents (0-52 at.% Co) were synthesized by a novel liquid ceramics method. The solubility limit for Co was determined at 550 degrees C. The lattice parameter c of the ZnO-based solid solution with wurzite structure ceases to grow at 33 at.% Co. The peaks of the second phase (Co2O3 or with cubic lattice) become visible in the X-ray diffraction spectra at 40 at.% Co. The same second phase appears in the bulk ZnO already at 2 at.% Co [Bates CH, White WB, Roy R. J Inorg Nucl Chem 1966;28:397]. A few years ago it was predicted theoretically that ZnO could become Ferromagnetic at room temperature and above by doping with Co and other transition metals. Recently published papers on the structure and magnetic behaviour of Co-doped ZnO allowed us to obtain the size dependence of CO Solubility in ZnO for the polycrystals and small single-crystalline particles. The overall Co Solubility drastically increases with decreasing grain size. The quantitative estimation leads to the conclusion that, close to the bulk solubility limit, the thickness of a Co-enriched layer is several monolayers in grain boundaries and at least two monolayers in the free surfaces. (C) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据