Preparation Sericite Nanoflakes by Exfoliation of Wet Ultrafine Grinding

出版社

TRANS TECH PUBLICATIONS LTD
DOI: 10.4028/www.scientific.net/AMR.178.242

关键词

sericite; nanoflakes; grind; exfoliation; shielding ultraviolet ray

资金

  1. National Natural Science Foundation [50674080]
  2. Beijing Natural Science Foundation [2032008]

向作者/读者索取更多资源

Sericite nanoflakes were prepared by exfoliating sericite layers by wet ultrafine grinding. Their appearance morphologies and main properties were characterized. Optimum conditions were studied with the purpose of forming shear stress which was beneficial to the exfoliation of mineral flakes. The results indicated that sericite nanoflakes could be prepared. Mass ratio of grinding media to materials, diameter ratio of grinding balls, solid content of powders and grinding time had significant effects on the preparation. The thicknesses of sericite nanoflakes were 20-80 nm, and the transmittances of ultraviolet ray with wavelength of 190-220 nm were only 0.1%-1%. This demonstrated that sericite nanoflakes had the function of shielding ultraviolet ray.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据