4.8 Article

Calcium phosphate deposition rate, structure and osteoconductivity on electrospun poly(L-lactic acid) matrix using electrodeposition or simulated body fluid incubation

期刊

ACTA BIOMATERIALIA
卷 10, 期 1, 页码 419-427

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.actbio.2013.08.041

关键词

Electrodeposition; SBF incubation; Calcium phosphate; Nanofiber; Bone tissue engineering

资金

  1. National Institutes of Health (NIDCR) [DE015384, DE017689, DE022327]
  2. DOD [W81XWH-12-2-0008]
  3. NSF [DMR-1206575]
  4. China Scholarship Council (CSC)/University of Michigan Post-Doctoral Program
  5. Division Of Materials Research
  6. Direct For Mathematical & Physical Scien [1206575] Funding Source: National Science Foundation

向作者/读者索取更多资源

Mineralized nanofibrous scaffolds have been proposed as promising scaffolds for bone regeneration due to their ability to mimic both nanoscale architecture and chemical composition of natural bone extracellular matrix. In this study, a novel electrodeposition method was compared with an extensively explored simulated body fluid (SBF) incubation method in terms of the deposition rate, chemical composition and morphology of calcium phosphate formed on electrospun fibrous thin matrices with a fiber diameter in the range similar to 200-1400 nm prepared using 6, 8, 10 and 12 wt.% poly(L-lactic acid) (PLLA) solutions in a mixture of dichloromethane and acetone (2:1 in volume). The effects of the surface modification using the two mineralization techniques on osteoblastic cell (MC3T3-E1) proliferation and differentiation were also examined. It was found that electrodeposition was two to three orders of magnitude faster than the SBF method in mineralizing the fibrous matrices, reducing the mineralization time from similar to 2 weeks to 1 h to achieve the same amounts of mineralization. The mineralization rate also varied with the fiber diameter but in opposite directions between the two mineralization methods. As a general trend, the increase of fiber diameter resulted in a faster mineralization rate for the electrodeposition method but a slower mineralization rate for the SBF incubation method. Using the electrodeposition method, one can control the chemical composition and morphology of the calcium phosphate by varying the electric deposition potential and electrolyte temperature to tune the mixture of dicalcium phosphate dihydrate and hydroxyapatite (HAp). Using the SBF method, one can only obtain a low crystallinity HAp. The mineralized electrospun PLLA fibrous matrices from either method similarly facilitate the proliferation and osteogenic differentiation of preosteoblastic MC3T3-E1 cells as compared to neat PLLA matrices. Therefore, the electrodeposition method can be utilized as a fast and versatile technique to fabricate mineralized nanofibrous scaffolds for bone tissue engineering. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.