The anti-calcification potential of a silsesquioxane nanocomposite polymer under in vitro conditions: Potential material for synthetic leaflet heart valve

期刊

ACTA BIOMATERIALIA
卷 6, 期 11, 页码 4249-4260

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.actbio.2010.06.015

关键词

Artificial heart valve; Calcification; Bioprostheses; Nanocomposite; Polymer

资金

  1. Engineering and Physical Sciences Research Council
  2. British Heart Foundation
  3. National Institute for Health Research
  4. National Institute for Health Research [J003] Funding Source: researchfish
  5. National Institutes of Health Research (NIHR) [J003] Funding Source: National Institutes of Health Research (NIHR)

向作者/读者索取更多资源

Calcification currently represents a major cause of failure of biological tissue heart valves. It is a complex phenomenon influenced by a number of biochemical and mechanical factors. Recent advances in material science offer new polymers with improved properties, potentially suitable for synthetic leaflets heart valves manufacturing. In this study, the calcification-resistance efficacy and mechanical and surface properties of a new nanocomposite polymeric material (polyhedral oligomeric silsesquioxane-poly(carbonate-urea)urethane; POSS-PCU) which has been developed by our group are assessed by means of in vitro testing. In particular, thin sheets of nanocomposite, glutaraldehyde-fixed bovine pericardium (BP) and polyurethane (PU) were exposed to a calcium solution into a specially designed in vitro accelerated physiological pulsatile pressure system for a period of 31 days and a total of 4 x 10(7) cycles. The samples were investigated for signs of calcification after exposure to calcium solution by means of X-ray, microscopic and chemical inspections. Mechanical and surface properties were also studied using stress-strain behaviour and surface morphology and hydrophobicity. Comparison shows that, in the experimental conditions, the level of calcification for the nanocomposite is considerably lower than for the fixed BP (p = 0.008) and PU samples (p = 0.015). Also, mechanical properties were unchanged in POSS-PCU, while there was a significant deterioration in PU samples (p<0.05). Hydrophobicity was significantly reduced in both the POSS-PCU and PU samples (p<0.0001). However, the POSS-PCU nanocomposite remained more hydrophobic than the PU sample (p<0.0001). Less platelet adhered to the POSS-PCU compared to the PU (p<0.0001). These results indicate that the use of this nanocomposite in synthetic leaflets heart valves may lead to potential advantages in terms of long-term performances and durability. (C) 2010 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.