4.8 Article

Hydroxyapatite whisker-reinforced polyetherketoneketone bone ingrowth scaffolds

期刊

ACTA BIOMATERIALIA
卷 6, 期 3, 页码 856-863

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.actbio.2009.08.004

关键词

Bone ingrowth scaffolds; Composite; Hydroxyapatite; Micro-computed tomography; Polyetheretherketone

资金

  1. Indiana 21st Century Research and Technology Fund
  2. US Army Medical Research and Materiel Command [W81XWH-06-1-0196]
  3. Peer Reviewed Medical Research Program [PR054672]

向作者/读者索取更多资源

Hydroxyapatite (HA) whisker-reinforced polyetherketoneketone (PEKK) bone ingrowth scaffolds were prepared and characterized. High levels of porosity (75-90%) and HA whisker reinforcement (0-40 vol %) were attained using a powder processing approach to mix the HA whiskers, PEKK powder and a NaCl porogen, followed by compression molding at 350-375 degrees C and particle leaching to remove the porogen. The scaffold architecture and microstructure exhibited characteristics known to be favorable for osteointegration. Scaffold porosity was interconnected with a mean pore size in the range 200-300 mu m as measured by micro-computed tomography HA whiskers were embedded within and exposed on the surface of scaffold struts, producing a microscale surface topography, shown by von Kossa staining and scanning electron microscopy Therefore. HA whisker-reinforced PEKK bone ingrowth scaffolds may be advantageous for orthopedic implant fixation, including interbody spinal fusion. (C) 2009 Acta Materialia Inc Published by Elsevier Ltd All rights reserved

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据