4.8 Article

Self-reinforced composites of bioabsorbable polymer and bioactive glass with different bioactive glass contents. Part II: In vitro degradation

期刊

ACTA BIOMATERIALIA
卷 4, 期 1, 页码 156-164

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.actbio.2007.06.007

关键词

bioactive glass; composite; hydrolytic degradation; polylactide; self-reinforced

向作者/读者索取更多资源

The in vitro degradation behavior of self-reinforced bioactive glass-containing composites was investigated comparatively with plain self-reinforced matrix polymer. The materials used were spherical bioactive glass 13-93 particles, with a particle size distribution of 50125 mu m, as a filler material and bioabsorbable poly-L,DL-lactide 70/30 as a matrix material. The composites containing 0, 20, 30, 40 and 50 wt.% of bioactive glass were manufactured using twin-screw extruder followed by self-reinforcing. The samples studied were characterized determining the changes in mechanical properties, thermal properties, molecular weight, mass loss and water absorption in phosphate-buffered saline at 37 degrees C for up to 104 weeks. The results showed that the bioactive glass addition modified the degradation kinetics and material morphology of the matrix material. It was concluded that the optimal bioactive glass content depends on the applications of the composites. The results of this study could be used as a guideline when estimating the best filler content of other self-reinforced osteo-conductive filler containing composites which are manufactured in a similar way. (C) 2007 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据