4.6 Article

Electrochemical Deposition of Ni-W Crack-Free Coatings

期刊

COATINGS
卷 8, 期 7, 页码 -

出版社

MDPI
DOI: 10.3390/coatings8070233

关键词

Ni-W binary alloy; crack-free coatings; electrodeposition; pulse current mode; Faradic efficiency; pyrophosphate electrolyte

资金

  1. Ministry of Education and Science of the Russian Federation [11.9686.2017/8.9]

向作者/读者索取更多资源

The main features of electrochemical deposition of coatings based on Ni-W binary alloy in the pulse current mode using pyrophosphate electrolytes were studied. Two electrolytes with a pH of 8.7 and 9.5 were used. The deposition was carried out with the current density varying in the range of 0.01-0.1 A center dot cm(-2), and the duty cycle (the relative pulse duration) was changed within the range 20-100%. The surface morphology and elemental and phase composition of the coatings were studied by scanning electron microscopy, energy-dispersive X-ray microanalysis and X-ray diffractometry. The experimental conditions allowing us to achieve the maximum Faradaic efficiency and W content in the coatings were determined. It was found that the pulse current mode enabled the fabrication of crack-free coatings with a thickness greater than 6 mu m.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据