In order to investigate the microstructure evolution under high strain rate deformation of magnesium alloy, AZ31B magnesium alloy was impacted by Split Hopkinson Pressure Bar within the strain rates of 496s(-1) to 2120s(-1), then the specimens were observed by optical microscopy. The results show that when the strain rate are relatively low (496s(-1)-964s(-1)), the microstructure is predominated by high density of twinning, while increase the strain rate to 2120s(-1) the volume fraction of twins is decreased. This implies that at relatively lower strain rate the deformation mechanism of AZ31B magnesium alloy under impact loading is twinning; increasing the strain rate the prismatic slip and pyramidal slip may be active besides twinning.