4.6 Article

Effect of the Microstructure and Distribution of the Second Phase on the Stress Corrosion Cracking of Biomedical Mg-Zn-Zr-xSr Alloys

期刊

MATERIALS
卷 11, 期 4, 页码 -

出版社

MDPI
DOI: 10.3390/ma11040551

关键词

biodegradable; magnesium alloys; microstructure; second phase; stress corrosion cracking

资金

  1. Science and Technology Planning Project of Guangdong Province [2017B090903005]
  2. Science and Technology Planning Project of Guangzhou [201704030045]
  3. Jinan University [88015139, JNIWRM2017002]
  4. Fundamental Research Funds for the Central Universities [17817024]

向作者/读者索取更多资源

The stress corrosion cracking (SCC) properties of the bi-directional forged (BDF) Mg-4Zn-0.6Zr-xSr (ZK40-xSr, x = 0, 0.4, 0.8, 1.2, 1.6 wt %) alloys were studied by the slow strain rate tensile (SSRT) testing in modified simulated body fluid (m-SBF). The average grain size of the BDF alloys were approximately two orders of magnitude smaller than those of the as-cast alloys. However, grain refinement increased the hydrogen embrittlement effect, leading to a higher SCC susceptibility in the BDF ZK40-0/0.4Sr alloys. Apart from the grain refinements effect, the forging process also changed the distribution of second phase from the net-like shape along the grain boundary to a uniformly isolated island shape in the BDF alloys. The SCC susceptibility of the BDF ZK40-1.2/1.6Sr alloys were lower than those of the as-cast alloys. The change of distribution of the second phase suppressed the adverse effect of Sr on the SCC susceptibility in high Sr-containing magnesium alloys. The results indicated the stress corrosion behavior of magnesium alloys was related to the average grain size of matrix and the distribution and shape of the second phase.