4.7 Article

Selective leaching of nickel and cobalt from limonitic laterite using phosphoric acid: An alternative for value-added processing of laterite

期刊

JOURNAL OF CLEANER PRODUCTION
卷 189, 期 -, 页码 620-626

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.jclepro.2018.04.083

关键词

Limonitic laterite; Phosphoric acid; Atmospheric leaching; Selective leaching; Iron phosphate

资金

  1. National Natural Science Foundation of China [51234008]
  2. Co-Innovation Center for Clean and Efficient Utilization of Strategic Metal Mineral Resources

向作者/读者索取更多资源

Atmospheric acid leaching has advantages of low energy consumption and operating cost, compared with high pressure acid leaching of low-nickel limonitic laterites. However, it suffers low nickel recovery, low leaching selectivity of nickel/cobalt over iron and excessive waste generation. In this work, a new method was used for selective leaching of nickel and cobalt, as well as for preparing iron phosphate intermediate material by atmospheric phosphoric acid leaching of limonitic laterite. The results show that 98.7% of nickel and 89.8% of cobalt are leached from the calcined limonitic laterite under optimized leaching conditions; meanwhile, 98.3% of iron is converted into insoluble FePO4 center dot 2H(2)O, resulting in the selective leaching of nickel and cobalt over iron. The leaching precipitate of FePO4 center dot 2H(2)O has a purity of 94%, which is expected to be a high-value by-product, providing an extra economic value. This work presents an alternative for value-added processing of laterite, featured by high leaching efficiency of nickel and cobalt without generation of solid waste. (C) 2018 Elsevier Ltd. All rights reserved.