4.5 Article

Development of electrospun poly (vinyl alcohol)-based bionanocomposite scaffolds for bone tissue engineering

期刊

JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A
卷 106, 期 4, 页码 1111-1120

出版社

WILEY
DOI: 10.1002/jbm.a.36309

关键词

electrospinning; PVA bionanocomposites; scaffolds; bone tissue engineering; cell culture

资金

  1. European Regional Development Fund within the Operational Program Innovative Economy

向作者/读者索取更多资源

The article is focused on the role of nanohydroxy apatite (nHAp) and cellulose nanofibers (CNFs) as fillers in the electrospun poly (vinyl alcohol) (ES-PVA) nanofibers for bone tissue engineering (TE). Fibrous scaffolds of PVA, PVA/nHAp (10 wt.%), and PVA/nHAp(10 wt.%)/CNF(3 wt.%) were successfully fabricated and characterized. Tensile test on electrospun PVA/nHAp10 and PVA/nHAp10/CNF3 revealed a three-fold and seven-fold increase in modulus compared with pure ES-PVA (45.45 +/- 4.77). Although, nanofiller loading slightly reduced the porosity percentage, all scaffolds had porosity higher than 70%. In addition, contact angle test proved the great hydrophilicity of scaffolds. The presence of fillers reduced in vitro biodegradation rate in PBS while accelerates biomineralization in simulated body fluid (SBF). Furthermore, cell viability, cell attachment, and functional activity of osteoblast MG-63 cells were studied on scaffolds showing higher cellular activity for scaffolds with nanofillers. Generally, the obtained results confirm that the 3-componemnt fibrous scaffold of PVA/nHAp/CNF has promising potential in hard TE. (c) 2018 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 106A: 1111-1120, 2018.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据