4.3 Article

Electrospun polycaprolactone/gelatin/bioactive glass nanoscaffold for bone tissue engineering

出版社

TAYLOR & FRANCIS AS
DOI: 10.1080/00914037.2018.1482461

关键词

Bioactivity; bone tissue engineering; degradation behavior; electrospun scaffold; mechanical properties; nanocomposite

向作者/读者索取更多资源

Polycaprolactone scaffolds, polycaprolactone/gelatin, and polycaprolactone/gelatin/bioactive glass scaffolds were prepared with ratios of 50/50, 25/75, and 75/25 for polymers and 5 wt% for the bioactive glass via electrospinning and then were characterized using. The results indicated that by adding gelatin and bioactive glass to polycaprolactone scaffold, the diameter of fiber decreased from 557 to 167 nm. The results showed growth of apatite layer on the scaffolds after immersion in simulated body fluid for 28 days. The results of mechanical test revealed that by adding bioactive glass to scaffolds, the ultimate tensile strength and Young's modulus increase about two folds.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据