Due to problems with most of the existing conservation treatments, new materials for the stabilization of waterlogged archaeological wood are highly desirable. The ideal consolidant should be environmentally friendly and safe to work with for conservators, while strengthening the objects without ruining the visual impression of the wood or filling it in ways that prevent re-treatment in the future. This paper tests chitosan since it is a multifunctional material that not only offers support but also hinders catalytic activity by potentially chelating reactive metal ions. Three solutions of 2% chitosan in 0.1 M acetic acid were chosen as a consolidant for samples from a 1150-year-old piece of waterlogged Viking Age wood from Slagen prestegard. The penetration of chitosan was determined by freeze-drying the samples and analyzing them using high-performance liquid chromatography (HPLC). It was found that chitosan solution penetrated at least. cm into the wood along the grain over the span of. weeks. Depolymerizing the chitosan only improved uptake slightly. The chitosan left an open structure in the waterlogged archaeological wood. It offered some strength to severely degraded waterlogged wood, but further tests are needed to evaluate stability, shrinkage, and fixation.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据