4.7 Article

Thermally induced degradation of NaCMC in water and effects of NaHCO3 on acid formation and charge

期刊

FOOD HYDROCOLLOIDS
卷 74, 期 -, 页码 32-36

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.foodhyd.2017.07.028

关键词

NaCMC; Heat treatment; Degradation; Hydrolysis

资金

  1. Stora Enso Oyj

向作者/读者索取更多资源

High purity (>99.5%) NaCMC solution was heated in ion-exchanged water and in an aqueous 10 mM NaHCO3 buffer solution and studied as a function of time and temperature. The effects of thermal treatment on viscosity, pH, molecular weight and cationic demand of the solutions were measured. It was found that the anionic groups of carboxymethylcellulose are relatively stable against thermally induced degradation, but a reduction in NaCMC chain length and viscosity was observed. Only the highest applied temperature ( 177 degrees C), especially without any pH control, destroyed the side groups of the NaCMC. This was observed as a decrease in cationic demand and in the formation of glycolic acid. The application of buffer was noticed to retard the degradation of side groups. The observed decrease in viscosity with increasing reaction time in the presence of air was relatively well described by a second order reaction. (C) 2017 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据