期刊
EXPRESS POLYMER LETTERS
卷 12, 期 1, 页码 82-99出版社
BUDAPEST UNIV TECHNOL & ECON
DOI: 10.3144/expresspolymlett.2018.7
关键词
thermal properties; packaging plastic waste; polymeric mixtures; chemical recycling; pyrolysis kinetics
The thermal behavior and pyrolytic kinetic analysis of main waste polymers (polypropylene (PP), polyethylene film (PE), poly(ethylene terephthalate) (PET), polystyrene (PS)) and three synthetic mixtures representing commingled post-consumer plastics wastes (CPCPWs) output from material recovery facilities were studied. Thermogravimetry (TG) pyrolysis experiments revealed that the thermal degradation of single polymers and the synthetic mixture enriched in PP occurred in one single step. The other two mixtures underwent a two-consecutive, partially overlapping degradation steps, whose peaks related to the first-order derivative of TG were deconvoluted into two distinct processes. Further TG experiments carried out on binary mixtures (PS/PP, PET/PP, PET/PEfilm and PP/PEfilm) showed a thermal degradation reliance on composition, structure and temperatures of single polymer components. A kinetic analysis was made for each step using the Kissinger-Akahira-Sunose (KAS) method, thus determining almost constant activation energy (E-a) for pyrolysis of PS, PET, PP and PE film in the range 0.25
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据
© Peeref 2019-2024. All rights reserved.