4.7 Article

The post-breakage response of laminated heat-treated glass under in plane and out of plane loading

期刊

COMPOSITES PART B-ENGINEERING
卷 147, 期 -, 页码 227-239

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.compositesb.2018.04.005

关键词

Laminated glass; Post-glass-breakage response; Bending; Reinforced concrete; Polyeric interlayer; Tension stiffening

资金

  1. Italian Dipartimento della Protezione Civile under project ReLUIS-DPC
  2. Italian Ministero dell'Istruzione, dell'Universitei e della Ricerca under grant MIUR-PRIN voce COAN [5.50.16.01, 2015JW9NJT]

向作者/读者索取更多资源

Any reliable use of glass for structural purposes cannot neglect that its breakage may be provoked by imponderable events, like impacts at critical spots or thermal shocks. Laminated glass, composed by glass plies sandwiching polymeric interlayer sheets, is used in architectural application thanks to its safe post-glass breakage response. When glass breaks, the interlayer retains the glass shards, and the cracked element maintain a certain residual load-bearing capacity, strongly influenced by the tension stiffening of the polymer due to the adhesion with the glass shards, which depends upon the size of the shards and of the debonded zones. Here, we review the most recent experimental results on the post-glass breakage response of laminated heat-treated glass elements, providing charts for the evaluation of such a stiffening effect. Based on this, simple formulas to analyze and interpret the experimental findings under both in-plane and out-of plane bending are proposed, providing analogies with the bending of bimodulus materials and the load-bearing mechanism of reinforced concrete, respectively.