4.7 Article

The formation and properties of Sialon-ZrN composites produced by reaction bonding combined with post gas-pressure sintering

期刊

CERAMICS INTERNATIONAL
卷 44, 期 9, 页码 10753-10761

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.ceramint.2018.03.112

关键词

Sialon-ZrN composites; Gas-pressure sintering; Hardness; Fracture toughness

资金

  1. China Scholarship Council (CSC) [2013060400019]

向作者/读者索取更多资源

Sialon-ZrN composites have been fabricated by a combination of reaction bonding and post-gas-pressure sintering. Composites with different amount of ZrN were post sintered at 1600, 1700 and 1800 degrees C under a nitrogen pressure of 0.7 MPa for 6 h. The results showed that mass loss due to decomposition increased with increasing sintering temperature. The mass loss at 1600 and 1700 degrees C was comparable, and below 3% even for the highest ZrN content of 50 wt%, but ranged between 6% and 9% for samples post sintered at 1800 degrees C with 10-50 wt% ZrN. Composites sintered at 1700 degrees C had the highest relative density (> 97%) and lowest open porosity (< 2%), and this was independent of ZrN content. The incorporation of the ZrN particles was observed to have an effect on the mechanical properties of the composites. The highest hardness (16.05 +/- 0.17 GPa) was observed for the composite sintered at 1700 degrees C with 20 wt% ZrN but decreased with higher ZrN contents, due to a weak bonding between the ZrN particles and the Sialon matrix. The fracture toughness showed a continuous increase with increasing ZrN content, due to the effect of the weak bonding on toughening mechanisms such as crack branching, crack deflection and crack bridging. The highest fracture toughness (5.35 +/- 0.18 MPa m(1/2)) was observed for the composited sintered at 1700 degrees C with 50 wt% ZrN.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据