This study presents the influence of the calcined kaolinite content of calcined clays on the hydration of Limestone Calcined Clay Cements containing 50% of clinker (LC3-50). Above a calcined kaolinite content of 65% in calcined clay, further reaction of clinker is inhibited from 3 days onwards. Detail investigation indicates that this slowing down of clinker hydration is related to a significant refinement of pore connectivity. A limiting critical pore entry radius of 3-5 nm is reached, from which the porosity does not get further refined. The higher the calcined kaolinite content, the faster this refinement limit is reached. The formation of carboaluminate hydrates is also limited after reaching this refinement limit. As a consequence, the on-going reaction of meta kaolin impacts C-A-S-H, mainly affecting gel porosity, which is not well characterized by MIP.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据