This study was undertaken to develop a product that will potentially delay the progress of deterioration of acid-deteriorated historic leather. Acid-deteriorated leather samples were treated with a new formulation consisting of aluminium di(isopropoxide) acetoacetate ester chelate (aluminium alkoxide) and 5-ethyl-1-aza-3,7-dioxabicyclo-[3.3.0]octane (oxazolidine II). The leather samples were also treated with oxazolidine II and aluminium alkoxide separately to compare the effectiveness of these reagents against the new formulation. Untreated leather samples were used as a negative control. Acid-deteriorated leather samples treated with Cellugelw, aluminium alkoxide and the new formulation along with corresponding untreated leather samples were also subjected to accelerated ageing in order to investigate the longevity of the treated leather. The impact of the treatments and accelerated ageing was determined by measuring the hydrothermal stability of the leather and pH of the aqueous extract. The formulation showed a potential to provide the acid-deteriorated historic leather with long-term protection against an artificially-created acidic environment.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据