The role of powder layer thickness on the quality of SLM printed parts

期刊

出版社

ELSEVIER URBAN & PARTNER SP Z O O
DOI: 10.1016/j.acme.2018.01.015

关键词

Additive manufacturing; Inconel; Layer thickness; Selective laser melting

资金

  1. A*STAR Additive Manufacturing Centre (AMC) Initiative: Work Package 1 (High Temperature Materials Development for 3D Additive Manufacturing) [142680088]

向作者/读者索取更多资源

Achieving good mechanical properties as well as the dimensional accuracy and the smooth surface quality of selective laser melting printed parts with minimal post treatments are essential in additive manufacturing. In the present study, Inconel 718 samples with different powder layer thickness (20, 30, 40 and 50 mu m) were additively fabricated using 3D Systems ProX-300 machine. The results reveal that the lower the layer thickness, the denser and good dimensional accuracy were achieved. Marginally higher mechanical properties and micro hardness were also obtained at the lower thickness while the failure strain was still high. This can be explained through significant change in the microstructure due to different cooling rate and thermal cycles. In addition, the formation of gamma' and gamma '' intermetallic phases, which were well distributed in the matrix and grain boundaries, during heating/cooling, gave rise in the strengths. Fractography shows the plastic deformation band due to work hardening and the crack initiation sites at sub-micro/micro pores, lack of fusion areas and the boundary of unmelted particles. The study would guide engineers balance their options between the production rate and the building parts' quality. (C) 2018 Politechnika Wroclawska. Published by Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据