Cutting efficiency of diamond burs operated with electric high-speed dental handpiece on zirconia

期刊

EUROPEAN JOURNAL OF ORAL SCIENCES
卷 123, 期 5, 页码 375-380

出版社

WILEY-BLACKWELL
DOI: 10.1111/eos.12211

关键词

cutting efficiency; diamond burs; leucite; lithium disilicate; zirconia

资金

  1. JSPS KAKENHI [25462981]
  2. Grants-in-Aid for Scientific Research [25462981] Funding Source: KAKEN

向作者/读者索取更多资源

Zirconia-based dental restorations are becoming used more commonly. However, limited attention has been given to the difficulties experienced, concerning cutting, in removing the restorations when needed. The aim of the present study was to compare the cutting efficiency of diamond burs, operated using an electric high-speed dental handpiece, on zirconia (Zir) with those on lithium disilicate glass-ceramic (LD) and leucite glass-ceramic (L). In addition, evaluation of the cutting efficiency of diamond burs on Zir of different thicknesses was performed. Specimens of Zir were prepared with thicknesses of 0.5, 1.0, 2.0, and 4.0mm, and specimens of LD and L were prepared with a thickness of 1.0mm. Cutting tests were performed using diamond burs with super coarse (SC) and coarse (C) grains. The handpiece was operated at 150,000rpm with a cutting force of 0.9N. The results demonstrated that cutting of Zir took about 1.5- and 7-fold longer than cutting of LD and L, respectively. The SC grains showed significantly higher cutting efficiency on Zir than the C grains. However, when the thickness of Zir increased, the cutting depth was significantly decreased. As it is suggested that cutting of zirconia is time consuming, this should be taken into consideration in advance when working with zirconia restorations.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.1
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据