Impact dynamics and energy dissipation capacity of fibre-reinforced self-compacting concrete plates

期刊

CONSTRUCTION AND BUILDING MATERIALS
卷 138, 期 -, 页码 383-397

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2017.02.011

关键词

Impact test; SCC; Fibre; Effective impact force; Energy dissipation capacity; Coefficient of restitution

向作者/读者索取更多资源

Applications of self-compacting concrete (SCC) in mega constructions have become increasingly popular. However, structures constructed with brittle SCC are extremely vulnerable to impact loading. Fibre reinforced SCC (FR-SCC) could be a viable solution to this problem, since the dynamic cracking in the SCC matrix can be restrained by the dispersed fibres and the overall impact resistance can be enhanced. However, the dynamics and failure mechanisms of FR-SCC subjected to impact loading are seldom explored in the literature. Furthermore, an excessive amount of fibres can deprive SCC of its favourable fluidity and segregation resistance. Hence, the fibre content has to be optimised to strike a balance between impact resistance and fluidity. In this regard, this paper presents a study on the impact dynamics of plates made of one SCC and three fibre-reinforced SCC (FR-SCC) mixes with different fibre content using a drop-weight testing apparatus. The rheological properties of the mixes were also investigated. The kinematic responses, effective impact forces, energy dissipation capacities, momentum transfer, and coefficients of restitution of the plates subjected to impact loading were evaluated and compared to explore the impact mechanisms. On the basis of the experimental results, the relationships between the effective impact forces and coefficients of restitution with the accumulated damage were obtained. The momentum transfer and impact duration remained approximately constant for the FR-SCC plates after being subjected to certain numbers of blows on account of the crack-bridging toughening mechanism. Also, it was found that the impact resistances and the energy dissipation capacities of the FR-SCC plates can be significantly higher than that of pure SCC plates by 6-14 times. (C) 2017 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据