High Tolerance to Iron Contamination in Lead Halide Perovskite Solar Cells

期刊

ACS NANO
卷 11, 期 7, 页码 7101-7109

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsnano.7b02734

关键词

photovoltaics; methylammonium lead iodide; extrinsic defects; impurities; photoluminescence; hysteresis; recombination

资金

  1. TOTAL S.A. through the MIT Energy Initiative
  2. MRSEC Program of the National Science Foundation (NSF) [DMR-1419807]
  3. U.S. Department of Energy's (DOE) Office of Energy Efficiency and Renewable Energy
  4. U.S. DOE Office of Science User Facility [DE-AC02-06CH11357]
  5. NSF under NSF EECS Award [1541959]
  6. Martin Family Society of Fellows for Sustainability
  7. Magdalene College, Cambridge
  8. Center for Excitonics, an Energy Frontier Research Center (EFRC) - U.S. DOE, Office of Science, Office of Basic Energy Sciences [DE-SC0001088]
  9. Center for Next Generation Materials by Design (CNGMD), an EFRC - U.S. DOE, Office of Science, Basic Energy Sciences [DE-AC36-08GO28308]
  10. NSF [1605406]
  11. DOE under NSF CA [EEC-1041895]
  12. NSF Graduate Research Fellowship [1122374]
  13. Directorate For Engineering
  14. Div Of Chem, Bioeng, Env, & Transp Sys [1605406] Funding Source: National Science Foundation

向作者/读者索取更多资源

The relationship between charge-carrier lifetime and the tolerance of lead halide perovskite (LHP) solar cells to intrinsic point defects has drawn much attention by helping to explain rapid improvements in device efficiencies. However, little is known about how charge-carrier lifetime and solar cell performance in LHPs are affected by extrinsic defects (i.e., impurities), including those that are common in manufacturing environments and known to introduce deep levels in other semiconductors. Here, we evaluate the tolerance of LHP solar cells to iron introduced via intentional contamination of the feedstock and examine the root causes of the resulting efficiency losses. We find that comparable efficiency losses occur in LHPs at feedstock iron concentrations approximately 100 times higher than those in p-type silicon devices. Photoluminescence measurements correlate iron concentration with nonradiative recombination, which we attribute to the presence of deep-level iron interstitials, as calculated from first-principles, as well as iron-rich,particles detected by synchrotron-based X-ray fluorescence microscopy. At moderate contamination levels, we witness prominent recovery of device efficiencies to near-baseline values after biasing at 1.4 V for 60 s in the dark. We theorize that this temporary effect arises from improved charge-carrier collection enhanced by electric fields strengthened from ion migration toward interfaces. Our results demonstrate that extrinsic defect tolerance contributes to high efficiencies in LHP solar cells, which inspires further investigation into potential large-scale manufacturing cost savings as well as the degree of overlap between intrinsic and extrinsic defect tolerance in LHPs and perovskite-inspired lead-free stable alternatives.