Hydrothermal Steel Slag Valorization-Part II: Hydrogen and Nano-Magnetite Production

期刊

FRONTIERS IN EARTH SCIENCE
卷 5, 期 -, 页码 -

出版社

FRONTIERS MEDIA SA
DOI: 10.3389/feart.2017.00086

关键词

magnetite; nanoparticles; BOF steel slag; hydrothermal oxidation; hydrogen production

资金

  1. CNRS through the MissionInterdisciplinaire: Defi Transition Energetique: Ressources, Societe, Environnement-ENRS program
  2. SATT Linksium (Grenoble)
  3. LabexOSUG@

向作者/读者索取更多资源

The effect of acidic conditions (in a pH range of 3 to 6) and temperature on the kinetics of the hydrothermal oxidation of ferrous iron contained in BOF steel slag has been tested in the 150-350 degrees C range for acid acetic concentrations from 0 to 4M. Reaction progress was monitored with the amount of produced H-2. Higher temperature and lower pH are found to enhance the hydrothermal oxidation kinetics of the slag. These two parameters are believed to increase iron dissolution rate which has already been identified as the rate limiting step of the hydrothermal oxidation of pure FeO. An activation energy of 28 +/- 4 kJ/mole is found for the hydrothermal oxidation of the steel slag which compares very well with that of pure FeO under similar conditions. In the case of the slag run in water at 300 degrees C for 70.5 h, magnetite product has been separated magnetically and characterized. Particles were found to fall in three size ranges: 10-30 nm, 100-300 nm, and 1-10 mu m. The smallest fraction (10-30 nm) is comparable to the 10-20 nm size range that is achieved when nanomagnetite are synthesized by co-precipitation methods. Obviously, the production of nanomagnetite enhances the economic interest of the hydrothermal processing of steel slags, which has already proven its capacity to produce high-purity H-2.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据