Effect of different curing regimes and durations on early strength development of reactive powder concrete

期刊

CONSTRUCTION AND BUILDING MATERIALS
卷 154, 期 -, 页码 72-87

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2017.07.181

关键词

Reactive powder concrete; Hot air curing; Hot water bath curing; Accelerated curing; Microstructure

向作者/读者索取更多资源

The early strength development of Reactive Powder Concrete (RPC) has been investigated under different curing regimes and compared with standard water curing condition. Four different curing regimes have been considered: ambient air curing, hot air curing, hot water bath curing and accelerated curing. The effect of hot air curing on strength development of RPC at different temperatures and durations are studied in detail. The present study is focused on the effect of combined curing regimes on the early strength development of RPC. Test results indicate that, among the four different curing regimes, hot water bath curing gives higher strength. The combined curing regime has considerably enhanced the compressive strength of RPC by about 63% as is evident by the rise in compressive strength from 110 MPa (standard curing) to 180 MPa (combined curing). Microstructure studies were also conducted to understand the arrangements of hydrated particles and development of other secondary hydrated products under different curing conditions using scanning electron microscope and X-ray diffraction spectroscopy respectively. (C) 2017 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据