Experiments were conducted to investigate the processing parameters that may be used to optimize the properties of Ti-6Al-4V alloys. The alloy was initially subjected to two different heat treatments leading to the formation of martensitic alpha' and lamellar alpha+beta microstructures and then both materials were processed by high-pressure torsion (HPT) for 10 turns at room temperature. This gave significant grain refinement to the nanometer range in both conditions and the occurrence of an allotropic hcp to fcc phase transformation in the martensitic alloy. These nanostructured alloys were subjected to post deformation annealing (PDA) at temperatures in the range of 473-1023 K. The results show the hardness increases slightly to 773 K due to alpha'+fcc ->alpha+beta+fcc and alpha ->alpha+beta phase transformations in the martensitic alpha' and lamellar alpha+beta alloys and then decreases up to 1023 K due to recrystallization and grain growth. An optimum property of a very high yield strength (similar to 1120 MPa) and ultimate tensile strength (similar to 1200 MPa), together with excellent ductility (elongation to failure of similar to 26%), was achieved in the Ti-6Al-4V martensitic alloy processed by a combination of HPT followed by PDA at 873 K for 60 min. (C) 2017 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据