4.8 Article

Stabilizing Nanosized Si Anodes with the Synergetic Usage of Atomic Layer Deposition and Electrolyte Additives for Li-Ion Batteries

期刊

ACS APPLIED MATERIALS & INTERFACES
卷 7, 期 25, 页码 13801-13807

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsami.5b01853

关键词

silicon; anode; lithium battery; composite; carbon; additive

资金

  1. Ministry of Science and Technology (MOST) [103-2221-E-011-156-MY3, 103-3113-E-011-001, 101-3113-E-011-002, 101-2923-E-011-001-MY3]
  2. Ministry of Economic Affairs (MOEA) [101-EC-17-A-08-S1-183]
  3. Top University Projects of Ministry of Education (MOE) [100H451401]

向作者/读者索取更多资源

A substantial increase in charging capacity over long cycle periods was made possible by the formation of a flexible weblike network via the combination of Al2O3 atomic layer deposition (ALD) and the electrolyte additive vinylene carbonate (VC). Transmission electron microscopy shows that a weblike network forms after cycling when ALD and VC were used in combination that dramatically increases the cycle stability for the Si composite anode. The ALD-VC combination also showed reduced reactions with the lithium salt, forming a more stable solid electrolyte interface (SEI) absent of fluorinated silicon species, as evidenced by X-ray photoelectron spectroscopy. Although the bare Si composite anode showed only an improvement from a 56% to a 45% loss after 50 cycles, when VC was introduced, the ALD-coated Si anode showed an improvement from a 73% to a 11% capacity loss. Furthermore, the anode with the ALD coating and VC had a capacity of 630 mAh g(-1) after 200 cycles running at 200 mA g(-1), and the bare anode without VC showed a capacity of 400 mAh g(-1) after only 50 cycles. This approach can be extended to other Si systems, and the formation of this SEI is dependent on the thickness of the ALD that affects both capacity and stability.