4.7 Article

Terminal group effects of phosphazene-triazine bi-group flame retardant additives in flame retardant polylactic acid composites

期刊

POLYMER DEGRADATION AND STABILITY
卷 140, 期 -, 页码 166-175

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymdegradstab.2017.04.024

关键词

Flame retardant; Polylactic acid; Synergistic effect; Phosphazene; Triazine

资金

  1. National Nature Science Foundation [51503008, 51403007]
  2. National Key RD Program [2016YFB0302104]

向作者/读者索取更多资源

Three phosphazene-triazine bi-group flame retardant additives (Al, A2, A3) with different terminal groups were synthesized from hexachlorocyclotriphosphazene (HCCP), cyanuric chloride and amine compounds (ethylenediamine, aniline, or p-phenylenediamine). Then they were applied with ammonium polyphosphate (APP) to prepare flame-retardant polylactic acid (PIA), separately. The molecule structures and thermal stabilities of these three flame retardant additives were characterized by Fourier transformed infrared spectrometry (FTIR), H-1 and C-13 Solid-State NMR spectrometer and thermogravimetric analysis (TGA). The flame-retardant properties and mechanism of the flame-retardant PLA composites were investigated by the limited oxygen index (LOI) test, vertical burning test, cone calorimeter test (CCT), scanning electron microscopy (SEM), and thermogravi-metric analyzer coupled to a Fourier-transform infrared spectrometer (TGA-FTIR). Results showed that the combination of phosphazene-triazine bi-group flame retardant additive with amino-terminated groups (Al or A3) and APP brought better flame retardant properties to PIA resin than that of A2 without amino -terminated groups. PLA/Al/APP system got the best flame retardant properties, which exhibited the highest LOI value of 34.3% and preferably achieved UL-94 V-0 rating without dripping. Meanwhile, it not only obtained the lowest plc-HRR, THR, and TSR, but also reserved the largest amount of residual char, compared with other flame-retardant PLA composites. Such a significant improvement in flame retardancy was attributed to the PO2 radical quenching effect and inert gas dilution effect in gas phase, as well as barrier and protective effect and charring effect in condense phase. Besides, the poor performance on flame retardancy of PLA/A2/APP system was due to the lack of barrier and protective effect and charring effect in condense phase. All these revealed that the adjustment on terminal groups of flame-retardant additives not only affects their flame-retardant work mode, but also helps to explore the more efficient flame-retardant structures or systems. (C) 2017 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据