4.8 Article

Effects of graphene defects on gas sensing properties towards NO2 detection

期刊

NANOSCALE
卷 9, 期 18, 页码 6085-6093

出版社

ROYAL SOC CHEMISTRY
DOI: 10.1039/c7nr01120b

关键词

-

向作者/读者索取更多资源

The crystal structure of graphene flakes is expected to significantly affect their sensing properties. Here we report an experimental investigation on the crystalline structure of graphene aimed at exploring the effects on the gas sensing properties. The morphology of graphene, prepared via Chemical Vapor Deposition (CVD), Liquid Phase Exfoliation (LPE) and Mechanical Exfoliation (ME), is inspected through Raman spectroscopy, Atomic Force Microscopy (AFM) and Scanning Electron Microscopy (SEM). CVD and LPE-graphene structures are found to be more defective with respect to ME-graphene. The defects are due to the jagged morphology of the films rather than originating from intrinsic disorder. The flatness of ME-graphene flakes, instead, explains the absence of defects. Chemiresistors based on the three different graphene preparation methods are subsequently exposed to NO2 in the concentration range 0.1-1.5 ppm (parts per million). The device performance is demonstrated to be strongly and unambiguously affected by the material structure: the less defective the material is, the higher the response rate is. In terms of signal variation, at 1.5 ppm, for instance, ME-graphene shows the highest value (5%) among the three materials. This study, comparing simultaneously graphene and sensors prepared via different routes, provides the first experimental evidence of the role played by the graphene level of defectiveness in the interaction with analytes. Moreover, these findings can pave the path for tailoring the sensor behavior as a function of graphene morphology.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据