Deficiencies of Chemically Reduced Graphene as Electrode in Full Li-Ion Cells

期刊

ELECTROCHIMICA ACTA
卷 165, 期 -, 页码 365-371

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2015.03.039

关键词

Graphene-based anode; Li-ion battery; Full-cell configuration; Prelithiation; Precycling activation method; Contact activation method

资金

  1. Ministerio de Economia y Competitividad [MAT2011-27110]
  2. Junta de Andalucia (Group FQM-175)

向作者/读者索取更多资源

In spite of the good electrochemical performance of graphene as electrode vs. lithium (half-cell configuration), graphene does not work in a full Li-ion cell as the delivered capacity continuously fades on cycling. The high irreversible capacity (IC) of the electrode observed in the former configuration, which is caused by the solid-electrolyte interface (SEI) formation, can be one of the causes of this shortcoming. As a remedy to this drawback, the graphene electrode was subjected to a lithiation process to form the SEI before assembling the full cell. Two lithiation methods were implemented: 1) precycling the electrode vs. a Li foil, and 2) placing the electrode in contact with a Li foil that was wetted with the electrolyte. Both methods improved the performance of the full cell, particularly the contact treatment, but the capacity retention on cycling was moderate. Moreover, not only does the electrode activation govern the electrochemical response, but factors such as the synthesis method and particle dimensions can also affect the cell performance. (C) 2015 Published by Elsevier Ltd.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据