Fabrication of TiB2/Al composite by melt-SHS process with different content of titanium powder

期刊

JOURNAL OF MATERIALS RESEARCH
卷 32, 期 12, 页码 2352-2360

出版社

CAMBRIDGE UNIV PRESS
DOI: 10.1557/jmr.2017.184

关键词

TiB2; composite; SHS; oxide; titanium powder

向作者/读者索取更多资源

Melt-SHS (self-propagating high-temperature synthesis), based on the SHS process and oxide reaction method, was used for preparation of TiB2/Al composites. The mass ratio of two reactants, Ti powder/TiO2, in initial powder mixture was varied from 0:1 to 1:0. The results showed that the 5 wt% TiB2/Al composites could be successfully produced by a reaction of aluminum powder, TiO2, and B2O3 in Al melt at 950 degrees C, while the reaction rate was slow. The addition of titanium powder helps to reduce the content of Al2O3 and destroy the coating structure of Al2O3 covered TiB2 particles, which leads to the acceleration of reaction process and improvement of particle concentration. A significant improvement was that TiB2 particles were dispersively distributed when the mass ratio of Ti powder/TiO2 was 2:3. As a result, the 5 wt% TiB2/Al composites fabricated by melt-SHS process with modified reactants ratio showed excellent tensile properties with the ultimate tensile strength as high as 114.24 MPa. Besides, the composite also showed superior ductility.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据