The objective of this study was to investigate the effect of magnesium (1 wt%) and aluminum (1 wt%) incorporation on the in vitro bioactivity and biodegradation behavior of 45S5 bioactive glasses synthesized from rice husk biogenic silica. The performance of biogenic silica-based samples was compared well with commercial silica-based counterparts. The in vitro biodegradation behavior of bioactive glasses was evaluated by the weight loss of samples and pH variation in the Tris buffer solution. Based on composition, bioglasses possessed different properties before and after simulated body fluid (SBF) immersion. The incorporation of magnesium (Mg) and aluminum (Al) enhanced the Vickers hardness of bioglasses. All the bioglasses showed the hydroxyapatite layer formation after SBF treatment as confirmed by the dissolution, FTIR, SEM and XRD analysis, however it was more prominent in the rice husk silica-based 45S5 bioglass. The biogenic silica seems to be a promising starting material for bioglass systems to be used in bone tissue engineering applications.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据