SO2 deactivation mechanism of NO oxidation and regeneration of the LaCoO3 perovskite

期刊

CATALYSIS SCIENCE & TECHNOLOGY
卷 10, 期 7, 页码 2193-2202

出版社

ROYAL SOC CHEMISTRY
DOI: 10.1039/c9cy02478f

关键词

-

资金

  1. SINCHEM Grant
  2. Erasmus Mundus Action 1 Programme [FPA 2013-0037]

向作者/读者索取更多资源

The deactivation mechanism and methods to cope with the poisoning by SO2 of LaCoO3 perovskite-based NO oxidation catalysts were investigated. The LaCoO3 perovskite was synthesized by a sol-gel method and the fresh, sulphate-deactivated and regenerated catalysts were characterized by X-ray diffraction, X-ray photoelectron spectroscopy, H-2-and soot-temperature programmed reduction, temperature programmed desorption and diffuse reflectance infrared Fourier transform spectroscopy. The SO2 poisoning strongly affected the NO oxidation activity. It was demonstrated that the deactivation mechanism proceeds in two stages: initially the active sites with a basic character are blocked by SO3 and subsequently the lanthanum sulphate salts grow progressively on the surface and cobalt is unaffected. Above 500 degrees C, the surface bound sulphates become mobile and migrate into the bulk of the catalyst. Several prevention and regeneration methods were proposed and tested. By mixing the catalyst with Ca(OH)(2) as an adsorbent nearly 50% of the original activity was retained. Regeneration by diesel soot was presented here for the first time, where the blocking oxygen can spill over to the soot oxidizing it and releasing the bound sulphur as SO2 and CO2. Furthermore, a facile regeneration method was explored by washing the deactivated catalyst to dissolve the small amounts of sulphates on the surface.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据