Moderate Dilution of Copper Slag by Natural Gas

期刊

JOM
卷 70, 期 1, 页码 47-52

出版社

SPRINGER
DOI: 10.1007/s11837-017-2670-6

关键词

-

资金

  1. Basic Research Universities Special Fund Operations [N140204013, N130102002, N130702001]
  2. Education Department of Liaoning Province [LZ2014021]
  3. National Natural Science Foundation of China [51374064]

向作者/读者索取更多资源

To enable use of copper slag and extract the maximum value from the contained copper, an innovative method of reducing moderately diluted slag to smelt copper-containing antibacterial stainless steel is proposed. This work focused on moderate dilution of copper slag using natural gas. The thermodynamics of copper slag dilution and ternary phase diagrams of the slag system were calculated. The effects of blowing time, temperature, matte settling time, and calcium oxide addition were investigated. The optimum reaction conditions were identified to be blowing time of 20 min, reaction temperature of 1250A degrees C, settling time of 60 min, CaO addition of 4% of mass of slag, natural gas flow rate of 80 mL/min, and outlet pressure of 0.1 MPa. Under these conditions, the Fe3O4 and copper contents of the residue were 7.36% and 0.50%, respectively.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据