4.8 Article

Spatial dynamics of lithiation and lithium plating during high-rate operation of graphite electrodes

期刊

ENERGY & ENVIRONMENTAL SCIENCE
卷 13, 期 8, 页码 2570-2584

出版社

ROYAL SOC CHEMISTRY
DOI: 10.1039/d0ee01191f

关键词

-

资金

  1. U.S. Department of Energy (DOE) [DE-AC36-08GO28308]
  2. U.S. Department of Energy Vehicle Technology Office
  3. Royal Academy of Engineering [CiET1718\59]
  4. Faraday Institution under ISCF Faraday Challenge Fast Start project on Degradation of Battery Materials [EP/S003053/1 (FIRG001)]
  5. Faraday Institution under ISCF Faraday Challenge Fast Start project on Multi-scale Modelling [EP/S003053/1 (FIRG003)]
  6. EPSRC [EP/S003053/1] Funding Source: UKRI

向作者/读者索取更多资源

The principal inhibitor of fast charging lithium ion cells is the graphite negative electrode, where favorable conditions for lithium plating occur at high charge rates, causing accelerated degradation and safety concerns. The local response of graphite, both at the electrode and particle level, when exposed to fast charging conditions of around 6C is not well understood. Consequently, the conditions that lead to the onset of lithium plating, as well as the local dynamics of lithium plating and stripping, have also remained elusive. Here, we use high-speed (100 Hz) pencil-beam X-ray diffraction to repeatedly raster along the depth of a 101 mu m thick graphite electrode in 3 mu m steps during fast (up to 6C) charge and discharge conditions. Consecutive depth profiles from separator to current collector were each captured in 0.5 seconds, giving an unprecedented spatial and temporal description of the state of the electrode and graphite's staging dynamics during high rate conditions. The electrode is preferentially activated near the separator, and the non-uniformity increases with rate and is influenced by free-energy barriers between graphite's lithiation stages. The onset of lithium plating and stripping was quantified, occurring only within the first 15 mu m from the separator. The presence of lithium plating changed the behavior of the underlying graphite, such as causing co-existence of LiC6 and graphite in the fully discharged state. Finally, the staging behavior of graphite at different rates was quantified, revealing a high dependency on rate and drastic hysteresis between lithiation and delithiation.