Studies on alkali activated cements (AAC) of metakaolin (MK) with up to 50% replacement by limestone (LS) have recently emerged; although interesting, no reduction in the alkali content has generally been implemented, in detriment of the durability, safety, environmental impact and costs. This paper presents an innovative approach for designing sustainable AAC of composites precursors of MK with high contents of LS, activated by NaOH-Na2O center dot nSiO(2). The method combines design of mixtures and a multi-response statistical optimization, in which the 28-day strength was maximized while the CO2-emissions, energy demand and production cost were simultaneously minimized. The approach resulted in a binder with high LS and reduced MK and alkali contents. The optimal formulation was 80%LS, Na2O/Al2O3 = 0.94, and SiO2/Al2O3 = 3.54, equivalent to only 4.7% Na2O relative to the mass of the precursors (MK + LS), which reduces the risk of deleterious carbonation and is lower than the requirements of AAC of 100%MK and similar to those of AAC of blast furnace slag. This optimal binder had predicted and measured strengths of 49.96 +/- 13.1 and 51.9 +/- 0.7 MPa, respectively, which confirmed the accuracy of the modelling; its microstructure had a dense matrix of cementitious products with partially reacted limestone particles distributed throughout, the reaction products were amorphous with a chemical composition that suggested a mixture of (C,N) A-S-H with N-A-S-H, CASH and C-S-H. Compared to a reference portland cement, the optimal formulation emits 75.1% less CO2, consumes 41.1% less energy and is 42.6% less expensive; while compared to the AAC of 100%MK, the reductions were 51.6, 53.8 and 57.5%, respectively. The optimal formulation represents a competitive sustainable alternative cement. (C) 2020 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据